Polyurethane Anticorrosive Coating

This article is not an official document, it is based on personal experience and is a recommendation. The process of applying polyurethane anti-corrosion coating on the sdt (pipe fittings). In during the deposition of corrosion-resistant coating is necessary to observe safety rules and fire safety. Understanding Anti-corrosion coating designed for corrosion protection of steel exterior surface products. Coating, depending on the material produced by plants airless Graco high pressure, with pre-heated material.

Mixing two-component materials produced by volume according to the documentation on the cover. Coating components in its composition does not contain solvents. The process of curing is due to the polymerization reaction. Complete polymerization coating ends in a few days. At +20 C for the different types of coatings, it ranges from 5 to 7 days. Quality corrosion-resistant coating must comply technical conditions. Requirements for malaria / coating method airless spray with separate components on sdt allowed men over 18 years that have passed the preliminary medical examination and found fit to work on the profession's past induction training on occupational safety, industrial hygiene and fire safety, have the proper qualifications.

In the production of Works painters are obliged to use personal protective equipment. When applied in the chamber should be two painter. One painter produces a coating on the product. The second follows the hose helps move the base, will switch the taps mixing module, gives the team the third painter. A third of malaria during the coating follows the work of painting equipment for the teams of painters producing the coating.

This entry was posted in News and tagged . Bookmark the permalink.

Comments are closed.